Metallography and Failure Analysis

 

 

Photomicrograph showing copper braze material joining steel plate
(above) to white iron (below). Note cracking below adhesion line
through the white iron casting.

 

Our metallurgical services include cross-sectioning, mounting & polishing specimens for microscopical examination including grain structure, grain size, inclusion rating, depth of carburization, case depth and plating thickness. State of the art Image Analysis Systems coupled to our microscopes and stereo microscopes assure compliance to the latest ASTM standards. Metallographic examination is an important tool in failure analysis for evaluation of fracture initiation sites and fracture modes. Our failure analysis service includes examining failed components and determining the cause of failure.